ASTM B489-85(2003)
Historical Standard: ASTM B489-85(2003) Standard Practice for Bend Test for Ductility of Electrodeposited and Autocatalytically Deposited Metal Coatings on Metals
SUPERSEDED (see Active link, below)
ASTM B489
1. Scope
1.1 This practice covers a test procedure for determining the ductility of electrodeposited and autocatalytically deposited coatings on sheet or strip basis metals. The purpose of the test is to determine the resistance of metal coatings to cracking during distortion.
1.2 Test Methods E8 can be used if the coatings are too ductile and require mandrels too small to be practical.
1.3 This standard does not purport to address all of the safety problems, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.
ASTM Standards
B177 Guide for Engineering Chromium Electroplating
D1193 Specification for Reagent Water
E8 Test Methods for Tension Testing of Metallic Materials
Keywords
autocatalytic deposits; ductility tests; electrodeposits; Bend testing--coatings; Ductility--electrodeposited materials; Autocatalytic coatings; Cracking resistance; Decorative coatings; Electrodeposited coatings; Electroless coatings; Engineered electrodeposited coatings; Metallic coatings;
ICS Code
ICS Number Code 25.220.40 (Metallic coatings)